Alyuminiy lasan temperining tezkor detallari–2

Alyuminiy qotishma rulonni qayta ishlash Temper, sharing the second article
Aluminum coil H12 work-hardened to 1/4 qiyin
Aluminum coil H14 work-hardened to 1/2 qiyin
Aluminum coil H16 work-hardened to 3/4 qiyin
Aluminum coil H18 work-hardened to 4/4 qiyin, anavi, to'liq qotib qolgan;
Alyuminiy lasan H19 super qattiqlashtirilgan holat. The tensile strength of this material should be more than 10N/mm2 higher than that of the H18 state material;

alyuminiy lasan 1050 sovuq haddelenmiş
Alyuminiy bobini H22 qisman tavlanadi 1/4 qattiq ishdan keyin qattiq;
Alyuminiy bobini H24 qisman tavlanadi 1/2 qattiq ishdan keyin qattiq;
Alyuminiy bobini H26 qisman tavlanadi 3/4 qattiq ishdan keyin qattiq;
Alyuminiy bobini H28 qisman tavlanadi 4/4 qattiq ishdan keyin qattiq;
Alyuminiy lasan H32 ga barqarorlashtirilgan 1/4 qattiq ishdan keyin qattiq;
Alyuminiy lasan H34 stabilizatsiya qilingan 1/2 qattiq ishdan keyin qattiq;
Aluminum coil H36 is stabilized to 3/4 qattiq ishdan keyin qattiq;
Aluminum coil H38 stabilized to 4/4 qattiq ishdan keyin qattiq;